Table 1. Particle diameter and polydispersity index of yuja microcomplex after UH and HPH treatment

Homogenization formulation Conditions Size (μm) PDI
None treatment 5.91±0.10e 0.82±0.08c
Ultrasonic homogenization (UH) Amp 30% / 5 min 4.69±0.07d 0.34±0.02b
Amp 30% / 15 min 2.90±0.07c 0.23±0.03a
Amp 30% / 30 min 1.79±0.05a 0.19±0.03a
High pressure homogenization (HPH) 1,000 bar / 1 cycle 2.23±0.05b 0.22±0.05a
1,000 bar / 2 cycle 1.96±0.02a 0.21±0.02a
1,000 bar / 3 cycle 1.90±0.03a 0.15±0.11a
Different letters in the same column indicate a significant difference at p<0.05 (n=3).